Inkcazo emfutshane:

Izitena zeMagnesia dolomite zenziwe nge-high-purity kunye ne-dense magnesia kunye ne-sintered magnesia dolomite sand okanye i-dolomite sand njengezinto zokwenza izinto. Ngokmimandla yokusetyenziswa eyahlukeneyo, khetha umlinganiso ofanelekileyo we-MgO kunye neCaO, sebenzisa isibopheleli esine-anhydr, kunye nefom kubushushu obufanelekileyo. , Ukushisa okuphezulu.

Izitena zeMagnesia dolomite zinokuxhathisa ngamandla kwi-iron ephantsi kunye ne-alkalinity ephantsi yokucoca i-slag ngaphandle kwesithando somlilo, kwaye iyanceda ekutshabalaliseni nasekudibaniseni ukususa ukungcola kwisinyithi, kwaye inefuthe lokucoca intsimbi etyhidiweyo. Isetyenziswa kwizitena zesamente, izitena ze-magnesia dolomite zinobudlelwane obukhulu kunye nesamente yesinki, kulula ukuxhonywa eziko, kwaye zinobungqingqwa obufanayo.


Iinkcukacha Product

INKQUBO YEMVELISO

UKUPHAKELA NOKUTHUNYELWA KWEENQWELO

Iimpawu zemveliso

Inkcazo

Izitena zeMagnesia dolomite zenziwe nge-high-purity kunye ne-dense magnesia kunye ne-sintered magnesia dolomite sand okanye i-dolomite sand njengezinto zokwenza izinto. Ngokmimandla yokusetyenziswa eyahlukeneyo, khetha umlinganiso ofanelekileyo we-MgO kunye neCaO, sebenzisa isibopheleli esine-anhydr, kunye nefom kubushushu obufanelekileyo. , Ukushisa okuphezulu.

Izitena zeMagnesia dolomite zinokuxhathisa ngamandla kwi-iron ephantsi kunye ne-alkalinity ephantsi yokucoca i-slag ngaphandle kwesithando somlilo, kwaye iyanceda ekutshabalaliseni nasekudibaniseni ukususa ukungcola kwisinyithi, kwaye inefuthe lokucoca intsimbi etyhidiweyo. Isetyenziswa kwizitena zesamente, izitena ze-magnesia dolomite zinobudlelwane obukhulu kunye nesamente yesinki, kulula ukuxhonywa eziko, kwaye zinobungqingqwa obufanayo.

Iimbonakalo

Amandla oomatshini alungileyo kumaqondo obushushu aphezulu / uzinzo olomeleleyo lokukhwankqiswa kobushushu obushushu

Ukuxhathisa okugqwesileyo ekumiselweni kweekhemikhali / Ukuhamba ngobushushu obuphezulu / Ngaba unokucoca isinyithi

Ukusetyenziswa

Izitena zaseMagnesia dolomite zilungele iifanishi zokucoca iintsimbi ezingenasici. Umzekelo, isixhobo sokucoca ngaphandle kwesithando somlilo sisetyenziselwa enye imveliso yezitena zemagnesia-chrome. Uluhlu lwayo lwesicelo luya luye lwahluthwa ngakumbi njengemveliso eyenye yezitena zemagnesia-chrome, kwaye uluhlu lwesicelo salo lubanzi kwaye lubanzi. Isetyenziselwa ukwakhiwa kweziko le-AOD, iziko le-VOD kunye nelile.

Izalathi zomzimba kunye nezeMichiza

Igama lebrand / Iipropati

MD15

MD20

MD25

MD30

MD40

Ukuxinana kobuninzi (g / cm3)

3.03

3.03

3.03

3.03

3

Ukunyaniseka okubonakalayo (%)

13

12

12

13

13

Amandla okuBanda okuBandayo (MPa)

80

90

80

80

80

Ukutshintsha kweMigca esisigxina (%) @ 1,500 ℃ x 2hrs

-

-0.35

-

-0.61

-

Ukuphinda ubenakho ukuphinda ulayishe (℃) @ 0.2MPa

1700

1700

1700

1700

1700

Ukwenziwa kweMichiza (%)

MgO

80.3

76.3

70.3

66.3

56.3

CaO

17

21

27

31

41

Al2O3

0.5

0.5

0.5

0.5

0.5

YFOO3

0.7

0.7

0.7

0.7

0.7

SiO2

1.3

1.3

1.3

1.3

1.2

Inkqubo yokuvelisa

Ulawulo lomgangatho wezinto ezibonakalayo ezi-1 kubandakanya uvavanyo lomzimba kunye neekhemikhali.           
2.Crushing nokuguba izinto ekrwada ekrwada.
3. Ngokoshicilelo lweenkcukacha zabathengi olufunekayo ekuxubeni iMathiriyeli ekrwada.
Ukucinezela okanye ukubumba isitena esiluhlaza kuxhomekeke kwizinto ezahlukeneyo zokwenza izinto kunye nokuma kwezitena.
4.Yomisa izitena kwindawo yomisi.
5.Beka izitena kwitonela yeziko ukuze ubaswe ngumgangatho ophakamileyo ukusuka kwi-1300-1800 deg.
Isebe lolawulo lomgangatho liza kuhlola izitena ezigqityiweyo ezingafunekiyo.

Ukupakisha kunye nokuhambisa ngenqanawe

Ukupakisha ngokhuseleko lokupakisha ulwandle-ngaphandle
Ukuhanjiswa: ukulayishwa kwezinto zokupakisha ezigqityiweyo kumzi mveliso ngesitya seDoor toDoor   
Ngolwandle ifutha ipallet yamaplanga + ibhanti yeplastiki + yokugoqa ifilimu.


  • Egqithileyo
  • Okulandelayo:

  • Ulawulo lomgangatho wezinto ezibonakalayo ezi-1 kubandakanya uvavanyo lomzimba kunye neekhemikhali.           
    2.Crushing nokuguba izinto ekrwada ekrwada.
    3. Ngokoshicilelo lweenkcukacha zabathengi olufunekayo ekuxubeni iMathiriyeli ekrwada.
    Ukucinezela okanye ukubumba isitena esiluhlaza kuxhomekeke kwizinto ezahlukeneyo zokwenza izinto kunye nokuma kwezitena.
    4.Yomisa izitena kwindawo yomisi.
    5.Beka izitena kwitonela yeziko ukuze ubaswe ngumgangatho ophakamileyo ukusuka kwi-1300-1800 deg.
    Isebe lolawulo lomgangatho liza kuhlola izitena ezigqityiweyo ezingafunekiyo.

    Ukupakisha ngokhuseleko lokupakisha ulwandle-ngaphandle
    Ukuhanjiswa: ukulayishwa kwezinto zokupakisha ezigqityiweyo kumzi mveliso ngesitya seDoor toDoor   
    Ngolwandle ifutha ipallet yamaplanga + ibhanti yeplastiki + yokugoqa ifilimu.

    Bhala umyalezo wakho apha uze uyithumele kuthi

    Iindidi zemveliso

    Gxila ekuboneleleni ngesisombululo se-mong pu seminyaka emi-5.